Melted metal together (TIG), then Self Etch Primer
Date: 11/28/2013
Views: 6859
Newest Image
EAA SITE
Date: 08/23/2023
Views: 721181
Most Viewed Image
EAA SITE
Date: 08/23/2023
Views: 721181
First pass of Port top wingskin bond on 1.
The Internet service @ hangar Pilots lounge was down, (perhaps due to lack of paying bill by landlord).
Thus Alan and I don't have access to documented bonding on of the Starboard wing.
Oh well.
First pass Redux / flox will be mixed a lot thicker than what I used on the Starboard wing.
I prepared yellow Redux:
2 oz for wetting out (more than half of which I added flox)
4 oz / flox
4 oz / flox
3.75 oz / flox.
Y10-09-11