Date: 12/31/1969 Views: 3740
Date: 06/08/2011 Views: 5414
Date: 12/31/1969 Views: 6091
Date: 08/23/2023 Views: 818885
After scuff sanding the fuse, we wet it out with Aeropoxy / 30 minute, then after squeegeeing off most of the thin Q-Cel slurry, (sealed the foam), we troweled on a thicker Q-Cel mixture. Y10-11-11